Abstract: The structural analysis of the thermo-insulation brick and ceramic cover of the third boiler of the working Kaunas Powerstation was carried out. It has been determined that the brick whose thickness is ~ 63 mm after staying in the energetic boiler at high temperature (1200-1400 ° C) around 98,985h demonstrates structural deposition. During the mentioned process that causes adequate alternations, the increase or decrease of the chemical elements in the parts and layers of the ceramic brick and its cover has been observed. It depends on the distribution of temperature within the volume of the brick.
Keywords: ceramics, high temperature, thermo-insulation, structure, needle-shaped, brick
Cite this article: Darius Abraitis. ANALYSIS OF CERAMICS EXPOSED TO EROSIVE COMBUSTION ENVIRONMENT. Journal of International Scientific Publications: Materials, Methods & Technologies 3, 508-514 (2009). https://www.scientific-publications.net/en/article/1003508/
Back to the contents of the volume
© 2026 The Author(s). This is an open access article distributed under the terms of the
Creative Commons Attribution License https://creativecommons.org/licenses/by/4.0/, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited. This permission does not cover any third party copyrighted material which may appear in the work requested.
Disclaimer: The Publisher and/or the editor(s) are not responsible for the statements, opinions, and data contained in any published works. These are solely the views of the individual author(s) and contributor(s). The Publisher and/or the editor(s) disclaim any liability for injury to individuals or property arising from the ideas, methods, instructions, or products mentioned in the content.